NASA's 3D-printed superalloy can take the heat
GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.
NASA's 3D-printed superalloy can take the heat
by Brian Newbacher for GRC News
Washington DC (SPX) Apr 24, 2023
NASA has demonstrated a breakthrough in 3D printable high-temperature materials that could lead to stronger, more durable parts for airplanes and spacecraft.

A team of innovators from NASA and The Ohio State University detailed the characteristics of the new alloy, GRX-810, in a peer-reviewed paper published in the journal Nature.

"This superalloy has the potential to dramatically improve the strength and toughness of components and parts used in aviation and space exploration," said Dr. Tim Smith of NASA's Glenn Research Center in Cleveland, lead author of the Nature paper. Smith and his Glenn colleague Christopher Kantzos invented GRX-810.

Smith and his team employed time-saving computer modeling, as well as a laser 3D printing process that fused metals together, layer-by-layer, to create the new alloy. They used this process to produce the NASA logo pictured above.

GRX-810 is an oxide dispersion strengthened alloy. In other words, tiny particles containing oxygen atoms spread throughout the alloy enhance its strength. Such alloys are excellent candidates to build aerospace parts for high-temperature applications, like those inside aircraft and rocket engines, because they can withstand harsher conditions before reaching their breaking points.

Current state-of-the-art 3D printed superalloys can withstand temperatures up to 2,000 degrees Fahrenheit. Compared to those, GRX-810 is twice as strong, over 1,000 times more durable, and twice as resistant to oxidation.

"This new alloy is a major achievement," said Dale Hopkins, deputy project manager of NASA's Transformational Tools and Technologies project. "In the very near future, it may well be one of the most successful technology patents NASA Glenn has ever produced."

A team of contributors from Glenn, NASA's Ames Research Center in California's Silicon Valley, NASA's Marshall Space Flight Center in Huntsville, Alabama, and The Ohio State University co-authored the Nature paper.

GRX-810 was developed under NASA's Transformational Tools and Technologies project, with support from the agency's Game Changing Development Program.

Related Links
Aeronautics at NASA
Space Technology News - Applications and Research

Subscribe Free To Our Daily Newsletters
Tweet

RELATED CONTENT
The following news reports may link to other Space Media Network websites.
TECH SPACE
SwRI joins new NASA institute to qualify, certify additive manufacturing methods
San Antonio TX (SPX) Apr 19, 2023
Southwest Research Institute will contribute to a new NASA institute to improve understanding and enable rapid certification of metal parts created using advanced additive manufacturing (AM) techniques. The Institute for Model-based Qualification and Certification of Additive Manufacturing (IMQCAM) will work to improve computer models of additively manufactured metal parts and expand their utility in spaceflight applications. Additive manufacturing uses 3D printing or rapid prototyping to build an ... read more

TECH SPACE
EU agency calls for reduction in pesticide use

EU agency calls for reduction in pesticide use

China's space achievements transforming agriculture

France frog fair faces criticism

TECH SPACE
Textile treatment sets a futuristic trend for new electronic applications

Two qudits fully entangled

Why are the US and China fighting over chips?

Ultra-miniaturized non-classical light sources for quantum devices

TECH SPACE
Air Force pilots reach new program milestones in electric vertical takeoff and landing aircraft

Helicopter flight paths to reduced emissions

Boeing reports another loss in Q1, but confirms forecast

EU set to put greener aviation fuel in planes

TECH SPACE
Chinese EV dominance hastens end of petrol engine era

Thousands protest planned motorway in France

Demand for electric cars 'booming': IEA

Tesla shares rebound as it tweaks prices on luxury models

TECH SPACE
Argentina to pay for Chinese imports in yuan instead of dollars

UK's Cleverly to urge against isolating China

Signs of hope for China property market, but boom is over: analysts

Asian stocks mixed ahead of tech earnings results

TECH SPACE
World's 'oldest' tree able to reveal planet's secrets

Indigenous Brazilians demand more land reserves

EU lawmakers adopt ban on imports speeding deforestation

California's beetle-killed, carbon-storing pine forests may not come back

TECH SPACE
Astraea launches new satellite tasking capabilities with major satellite imagery providers

Remote sensing of urban green space published

A more precise model of the Earth's ionosphere

Transforming nature conservation with the power of satellite imagery

TECH SPACE
Subscribe Free To Our Daily Newsletters




The content herein, unless otherwise known to be public domain, are Copyright 1995-2026 - Space Media Network. All websites are published in Australia and are solely subject to Australian law and governed by Fair Use principals for news reporting and research purposes. AFP, UPI and IANS news wire stories are copyright Agence France-Presse, United Press International and Indo-Asia News Service. ESA news reports are copyright European Space Agency. All NASA sourced material is public domain. Additional copyrights may apply in whole or part to other bona fide parties. All articles labeled "by Staff Writers" include reports supplied to Space Media Network by industry news wires, PR agencies, corporate press officers and the like. Such articles are individually curated and edited by Space Media Network staff on the basis of the report's information value to our industry and professional readership. Advertising does not imply endorsement, agreement or approval of any opinions, statements or information provided by Space Media Network on any Web page published or hosted by Space Media Network. General Data Protection Regulation (GDPR) Statement Our advertisers use various cookies and the like to deliver the best ad banner available at one time. All network advertising suppliers have GDPR policies (Legitimate Interest) that conform with EU regulations for data collection. By using our websites you consent to cookie based advertising. If you do not agree with this then you must stop using the websites from May 25, 2018. Privacy Statement. Additional information can be found here at About Us.